dc.description.abstract |
Oxidation behaviour of the near α-titanium alloy IMI 834 was investigated over a range of temperatures, from 600-800°C, in air. Specimens were solution-treated in the α + β and β phase fields for 1 h and 1/2 h, respectively and cooled in air to room temperature. The solution treated samples were subjected to stabilization treatment at 700°C for 2 h, followed by cooling in air. Oxidation behaviour of these samples was studied from 600-800°C in air, for 50 h. The morphology of the scales formed was examined by SEM and the phases present in the scales were characterized by X-ray diffraction. While there was little oxidation at 600°C, the rate of oxidation increased at higher temperatures. In general, the rate of oxidation was found to be more in the α + β treated condition than that in the β treated one. The results are discussed in terms of the characteristics of the oxide film formed under different conditions. |
en_US |
dc.description.sponsorship |
Bulletin of Materials Science |
en_US |
dc.language.iso |
en |
en_US |
dc.publisher |
Indian Academy of Sciences |
en_US |
dc.relation.ispartofseries |
Issue 4;Volume 27 |
|
dc.subject |
Activation energy; |
en_US |
dc.subject |
Near α-titanium alloy IMI 834; |
en_US |
dc.subject |
Oxidation behaviour; |
en_US |
dc.subject |
Surface morphology; |
en_US |
dc.subject |
Thermogravimetric studies |
en_US |
dc.title |
Oxidation behaviour of the near α-titanium alloy IMI 834 |
en_US |
dc.type |
Article |
en_US |