Electrical conduction in the solid solution La1 -x Na x Co1 -x Nb x O3 (0·01 ≤x ≤ 0·99)

Show simple item record

dc.contributor.author Parkash, O.M.
dc.contributor.author Kumar, D.
dc.contributor.author Kumar, R.
dc.date.accessioned 2021-08-25T12:19:05Z
dc.date.available 2021-08-25T12:19:05Z
dc.date.issued 1988-05
dc.identifier.issn 09737669
dc.identifier.uri http://localhost:8080/xmlui/handle/123456789/1577
dc.description.abstract Scebeek coefficient and DC resistivity of the solid solution Lal _~Na~Col _~Nb~O3 (001 ~< x <~0-99) have been measured in the temperature range 300-900 K. Seebeck coefficient is positive for all compositionsover the temperature range of measurements. Conduction is due to 3d electrons of cobalt ions in the compositions with x~<0.60. Conduction occurs among localized sites for compositions with x >/0.70. en_US
dc.description.sponsorship Bulletin of Materials Science en_US
dc.language.iso en en_US
dc.publisher Springer India en_US
dc.relation.ispartofseries Issue 3;Volume 10
dc.subject Lanthanum cobaltate; en_US
dc.subject lanthanum sodium cobalt niobium oxide; en_US
dc.subject sodium niobate en_US
dc.title Electrical conduction in the solid solution La1 -x Na x Co1 -x Nb x O3 (0·01 ≤x ≤ 0·99) en_US
dc.type Article en_US